Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® FRPS Polyester Film, 142 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® FRPS Polyester Film, 142 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® FRPS is a lower shrinkage version of Melinex® S. Designed specifically for release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and handling propertiesInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 96.5 MPa
14000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 100 MPa
14500 psi
ASTM D882A
Film Elongation at Break, MD 140 %
140 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Coefficient of Friction, Dynamic 0.30
0.30
A-B; ASTM D1894
Film Tensile Strength at Break, MD 200 MPa
29000 psi
ASTM D882A
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 3.5 %

@Temperature 190 °C,
Time 300 sec
3.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Transmission, Visible 87 %
87 %
TLT; ASTM D1003
Copyright © lookpolymers.com All Rights Reserved