Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® D316 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® D316 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® D316 is a polyester film designed for the label industry, one side pretreated to promote adhesion to a wide variety of solventless, UV, EB, and thermal cured coatings.Adhesion promoting one sideHigh surface energy (45-48 dynes)Faster processing/label application speedsInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 140 %
140 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Coefficient of Friction, Dynamic 0.40
0.40
A-B; ASTM D1894
Film Tensile Strength at Break, MD 207 MPa
30000 psi
ASTM D882A
Film Tensile Strength at Break, TD 262 MPa
38000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 0.50 %

@Temperature 190 °C,
Time 300 sec
0.50 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 10070 in2/lb
Users viewing this material also viewed the following: