Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® AG2 Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® AG2 Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® AG2 is a clear polyester film coated on both sides for Anti-fog and Anti-glare performanceTypical Applications: Typical applications include disposable face shields, visors, and other temporary optical and industrial uses.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 150 %
150 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Film Tensile Strength at Break, MD 152 MPa
22000 psi
ASTM D882A
Film Tensile Strength at Break, TD 165 MPa
24000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.5 %

@Temperature 190 °C,
Time 300 sec
2.5 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 0.90 %
0.90 %
ASTM D1003
Transmission, Visible 96 %
96 %
TLT; ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 4475 in2/lb
50 Gauge
5035 in2/lb
400 Gauge
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved