DuPont Teijin Films Melinex® 618 Polyester Film, 1000 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 618 Polyester Film, 1000 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 618 is a super clear polyester film, pretreated on one side to promote adhesion. It is a high clarity, non-yellow base with excellent adhesion on the pretreated surface. Used for a wide range of display applications.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 200 %
200 %
ASTM D882A
Film Elongation at Break, TD 120 %
120 %
ASTM D882A
Film Tensile Strength at Break, MD 179 MPa
26000 psi
ASTM D882A
Film Tensile Strength at Break, TD 186 MPa
27000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.4 %

@Temperature 190 °C,
Time 300 sec
2.4 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003