Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 595 Polyester Film, 400 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 595 Polyester Film, 400 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 595 is a high clarity film that is one side pretreated to provide anti-charge protection and one side pretreated to promote adhesion to many solvent coating formulations. This film is excellent for color proof applications.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 96.5 MPa
14000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 96.5 MPa
14000 psi
ASTM D882A
Film Elongation at Break, MD 160 %
160 %
ASTM D882A
Film Elongation at Break, TD 120 %
120 %
ASTM D882A
Coefficient of Friction, Dynamic 0.45
0.45
A-B; ASTM D1894
Film Tensile Strength at Break, MD 193 MPa
28000 psi
ASTM D882A
Film Tensile Strength at Break, TD 255 MPa
37000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.6 %

@Temperature 190 °C,
Time 300 sec
1.6 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 190 °C,
Time 300 sec
1.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 0.50 %
0.50 %
ASTM D1003
Transmission, Visible 89 %
89 %
TLT; ASTM D1003
Descriptive Properties Value Comments
Color -0.04
a
2.84
b
96.24
L
Copyright © lookpolymers.com All Rights Reserved