DuPont Teijin Films Melinex® 301H Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 301H Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 301H is a coextruded film that is one side heat sealable and is able to accept many industrial coatings.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 96.5 MPa
14000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 89.6 MPa
13000 psi
ASTM D882A
Film Elongation at Break, MD 110 %
110 %
ASTM D882A
Film Elongation at Break, TD 80 %
80 %
ASTM D882A
Coefficient of Friction, Dynamic 0.45
0.45
A-B; ASTM D1894
Film Tensile Strength at Break, MD 179 MPa
26000 psi
ASTM D882A
Film Tensile Strength at Break, TD 193 MPa
28000 psi
ASTM D882A
Optical Properties Metric English Comments
Transmission, Visible 88.5 %

@Thickness 0.0305 mm
88.5 %

@Thickness 0.00120 in
TLT; ASTM D1003
88.6 %

@Thickness 0.0152 mm
88.6 %

@Thickness 0.000600 in
TLT; ASTM D1003
88.6 %

@Thickness 0.0203 mm
88.6 %

@Thickness 0.000800 in
TLT; ASTM D1003
88.7 %

@Thickness 0.0122 mm
88.7 %

@Thickness 0.000480 in
TLT; ASTM D1003