DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy

Category Polymer , Thermoplastic
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Surlyn®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Surlyn® SG201U NC010 Supergloss Molding Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn® SG201U is a modified ionomer resin for applications that require a high gloss, molded in color surface color surface finish directly from the mold. The material is weatherable, durable, and provides improved scratch and abrasion resistance. Surlyn® SG201U is an excellent, lower cost, more environmentally friendly alternative to painting.Information provided by DuPont.
Physical Properties Metric English Comments
Specific Gravity 1.043 g/cc
1.043 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.8 MPa
6500 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Flexural Modulus 1.139 GPa
165.2 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm

@Temperature -30.0 °C
5.00 ft-lb/in

@Temperature -22.0 °F
ASTM D256
6.41 J/cm

@Temperature 23.0 °C
12.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 0.0940 µm/m-°C

@Temperature 20.0 °C
0.0522 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 14.4 °C
58.0 °F
ASTM D648
Vicat Softening Point 190 °C
374 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 235 - 250 °C
455 - 482 °F
Mold Temperature 40.6 - 79.4 °C
105 - 175 °F
Drying Temperature <= 79.4 °C
<= 175 °F