Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Selar® PA 3426 Nylon Barrier Resin

Category Polymer , Thermoplastic , Nylon , Nylon, Barrier Film Copolymer
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Selar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Selar® PA 3426 Nylon Barrier Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Selar® PA 3426 is an amorphous nylon (polyamide) resin which exhibits superior transparency, good barrier properties to gases, water, solvents and essential oils and high temperature structural properties which make it suitable for consideration in a number of packaging applications. It can be processed on conventional extrusion and injection equipment designed to process nylon or polyolefin resins. It is available in the form of small, free flowing pellets in 25 kg (55 lb.) foil-lined bags or 750 kg. (1653 lb.) foil lined boxes. Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D1505
Oxygen Transmission 0.470 cc-mm/m²-24hr-atm
1.19 cc-mil/100 in²-24hr-atm
40% RH, 23°C
Viscosity 200000 cP

@Shear Rate 100 1/s,
Temperature 300 °C
200000 cP

@Shear Rate 100 1/s,
Temperature 572 °F
Mechanical Properties Metric English Comments
Flexural Modulus 2.80 GPa
406 ksi
at 50% RH; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
259 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
253 °F
ASTM D648
Glass Transition Temp, Tg 127 °C
261 °F
ASTM D3418
Processing Properties Metric English Comments
Processing Temperature 280 - 320 °C
536 - 608 °F
Recommended for injection molding.