DuPont Performance Polymers Zytel® HTN FR55G50NHLW BK046 Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN FR55G50NHLW BK046 Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
55% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Low Warpage and High Stiffness Zytel HTNFR55G50NHLW BK046 is a 50% glass reinforced flame retardant high performance polyamide resin with improved flow and low warInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0020 cm/cm
0.0020 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
DAM; ISO 527-1/-2
Elongation at Break 1.6 %
1.6 %
DAM; ISO 527-1/-2
Tensile Modulus 17.5 GPa
2540 ksi
DAM; ISO 527-1/-2
Flexural Strength 306 MPa
44400 psi
DAM; ISO 178
Flexural Modulus 16.6 GPa
2410 ksi
DAM; ISO 178
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
DAM; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.0 µm/m-°C
6.67 µin/in-°F
DAM; ISO 11359-1/-2
11.0 µm/m-°C

@Temperature 55.0 - 160 °C
6.11 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
14.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
7.78 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 38.0 µm/m-°C
21.1 µin/in-°F
DAM; ISO 11359-1/-2
36.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
Melting Point 298 °C
568 °F
DAM; first heat; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
DAM; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
DAM; IEC 60695-11-10
V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
DAM; IEC 60695-11-10
Descriptive Properties Value Comments
Part Marking Code >PA-GF50FR<
ISO 11469
>PPA-GF50FR<
SAE J1344
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
UL recognition UL
DAM