Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
DAM; ISO 1183
Water Absorption 3.0 %

@Thickness 2.00 mm
3.0 %

@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.30 %

@Thickness 2.00 mm
1.30 %

@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm
0.013 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.0 MPa
7830 psi
50%RH; ISO 527-1/-2
62.0 MPa
8990 psi
DAM; ISO 527-1/-2
Elongation at Break 17 %
17 %
DAM; Nominal; ISO 527-1/-2
>= 50 %
>= 50 %
50%RH; Nominal; ISO 527-1/-2
Elongation at Yield 4.5 %
4.5 %
DAM; ISO 527-1/-2
18 %
18 %
50%RH; ISO 527-1/-2
Tensile Modulus 1.70 GPa
247 ksi
50%RH; ISO 527-1/-2
2.40 GPa
348 ksi
DAM; ISO 527-1/-2
Flexural Modulus 1.44 GPa
209 ksi
50%RH; ISO 178
2.10 GPa
305 ksi
DAM; ISO 178
Charpy Impact Unnotched NB
NB
DAM; ISO 179/1eU
NB
NB
50%RH; ISO 179/1eU
4.00 J/cm²

@Temperature -30.0 °C
19.0 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
DAM; ISO 179/1eA
0.400 J/cm²
1.90 ft-lb/in²
50%RH; ISO 179/1eA
0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eA
0.350 J/cm²

@Temperature -30.0 °C
1.67 ft-lb/in²

@Temperature -22.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 110 µm/m-°C
61.1 µin/in-°F
DAM; ISO 11359-1/-2
90.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
50.0 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
160 µm/m-°C

@Temperature 55.0 - 160 °C
88.9 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
DAM; ISO 11359-1/-2
90.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
50.0 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
180 µm/m-°C

@Temperature 55.0 - 160 °C
100 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
Melting Point 218 °C
424 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
275 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
DAM; ISO 75-1/-2
Vicat Softening Point 181 °C
358 °F
DAM; 50°C/h 50N; ISO 306
Glass Transition Temp, Tg 65.0 °C
149 °F
DAM; 10°C/min; ISO 11357-1/-2
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Part Marking Code >PA612<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA612
ISO 1043
Special Characteristics Light stabilised or stable to light