Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® FE270046 BK267 Nylon 66  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® FE270046 BK267 Nylon 66  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced Polyamide 66 + Polyamide 6T/XTInformation provided by DuPont Performance Polymers
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
50%RH; ISO 527-1/-2
140 MPa
20300 psi
DAM; ISO 527-1/-2
Elongation at Break 3.1 %
3.1 %
DAM; ISO 527-1/-2
4.5 %
4.5 %
50%RH; ISO 527-1/-2
Tensile Modulus 6.00 GPa
870 ksi
50%RH; ISO 527-1/-2
7.50 GPa
1090 ksi
DAM; ISO 527-1/-2
Thermal Properties Metric English Comments
Melting Point 259 °C
498 °F
DAM; 10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Delivery Form Pellets
Regional Availability Europe
Near East/Africa