Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers VTR 8605 (GF-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers VTR 8605 (GF-S) Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationVTR 8605
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Ultimate 18.0 MPa
2610 psi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Elongation at Break 246 %
246 %
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Modulus of Elasticity 0.00102 GPa
0.148 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
100% Modulus 0.00630 GPa
0.914 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Compression Set 16 %

@Temperature 200 °C
16 %

@Temperature 392 °F
Method B, O-rings 22 hr at 200°C (Post Cured 2 hr at 232°C)
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -5.00 °C
23.0 °F
MDSC, postcured