Material Notes:
DuPont Vespel TP-8929 parts are specified for mechanical and thermal performance. TP-8929 parts offer low friction, dimensional stability, low outgassing, radiation resistance, and creep resistance. TP-8929 parts are produced from filled thermoplastic polInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 72.0 MPa

@Temperature 23.0 °C
10400 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 6.0 %

@Temperature 23.0 °C
6.0 %

@Temperature 73.4 °F
ASTM D638
Flexural Strength 96.0 MPa

@Temperature 23.0 °C
13900 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 0.00240 GPa

@Temperature 23.0 °C
0.348 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 1.37 J/cm

@Temperature 23.0 °C
2.57 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 63.0 µm/m-°C

@Temperature 23.0 - 150 °C
35.0 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 228
CTE, linear, Transverse to Flow 54.0 µm/m-°C

@Temperature 23.0 - 150 °C
30.0 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E 228
Deflection Temperature at 1.8 MPa (264 psi) 230 °C
446 °F
ASTM D648
Descriptive Properties Value Comments
Appearance Natural Color
Forms Shapes
Material Status Current
Region Available - Global Yes
RoHS Compliance Contact Manufacturer