DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)

Category Polymer , Thermoplastic , Polyester, TP , Polytrimethylene Terephthalate (PTT)
Manufacturer DuPont Performance Polymers
Trade Name Sorona®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength stifInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption at Saturation 0.080 %
0.080 %
Immersion 24h; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
ISO 527-1/-2
Tensile Modulus 6.50 GPa
943 ksi
ISO 527-1/-2
Flexural Strength 190 MPa
27600 psi
ISO 178
Flexural Modulus 5.80 GPa
841 ksi
ISO 178
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179/1eU
3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179/1eA
0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 89.0 µm/m-°C
49.4 µin/in-°F
ISO 11359-1/-2
Melting Point 227 °C
441 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 223 °C
433 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 19 %
19 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250
3.9

@Frequency 100 Hz
3.9

@Frequency 100 Hz
IEC 60250
Dielectric Strength 36.0 kV/mm
914 kV/in
IEC 60243-1
Dissipation Factor 0.0015

@Frequency 100 Hz
0.0015

@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 250 V
250 V
IEC 60112
Descriptive Properties Value Comments
Part Marking Code >PTT-GF15<
ISO 11469
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PTT-GF15
Users viewing this material also viewed the following: