DuPont Performance Polymers Neoprene 750 Polychloroprene  (discontinued **)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Neoprene 750 Polychloroprene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Main feature: Excellent flexibility. Principal uses include: Dipped goods, Thread (Non-woven fabrics), Adhesives (Contact, Cord, Construction, Pressure Sensitive).Solids content: 50%. Initial pH: 12.5. Surface tension: 40 dyne/cm. Polymer type: Medium gel. Emulsifying agent: Potassium salt of disproportionated resin. Slow crystallization rate.Wet Gel Properties: Very high tensile strength. High elongation. Medium cure rate. Low modulus.General Neoprene Latex Information: Neoprene latexes are aqueous colloidal dispersions of polychloroprene or of copolymers of chloroprene with other monomers such as methacrylic acid or 2,3-dichloro-1,3-butadiene. They are available in both anionic and nonionic surfactant systems. All neoprene latexes have a unique combination of inherent characteristics including excellent film formation; high cohesive strength without curing; elastomeric properties over a wide temperature range; and considerable resistance to degradation from chemical or environmental exposure. Uses include adhesives, binders, coatings, dipped goods, elasticized asphalt and concrete, and foam.Information provided by DuPont Dow Elastomers.This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Latex
1.23 g/cc
0.0444 lb/in³
Polymer
Brookfield Viscosity 10 cP
10 cP
#1 spindle; 6 rpm.
10 cP
10 cP
#1 spindle; 30 rpm.