Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Hytrel® HTR237BG BK320 TPC-ET  (Unverified Data**)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Hytrel® HTR237BG BK320 TPC-ET  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hytrel® HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal durometer hardness of 45D, is pigmented black with fine particle size carbon black and contains a general purpose stabilizer.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 220 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D <= 45
<= 45
ISO 868
Tensile Strength at Break 31.0 MPa

@Temperature 23.0 °C
4500 psi

@Temperature 73.4 °F
ISO 527 (1BA bar)
Tensile Stress 7.60 MPa

@Strain 10.0 %,
Temperature 23.0 °C
1100 psi

@Strain 10.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
Elongation at Break 309 %

@Temperature 23.0 °C
309 %

@Temperature 73.4 °F
ISO 527 (1BA bar)
Izod Impact, Notched (ISO) NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ISO 180/1A
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point 199 °C
390 °F
10°C/min; ISO 11357-1/-3
Brittleness Temperature -100 °C
-148 °F
ISO 974
Glass Transition Temp, Tg -45.0 °C
-49.0 °F
10°C/min; ISO 11357-1/-2
Processing Properties Metric English Comments
Drying Temperature 110 °C
230 °F
Blow Molding
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Blow Molding
Moisture Content <= 0.020 %
<= 0.020 %
Blow Molding
Descriptive Properties Value Comments
Appearance Black Color
Forms Pellets
Generic TPC-ET
Material Status Preliminary Data
Part Marking Code >TPC-ET<
ISO 11469
Processing Method Blow Moldable
Product Category Blow Moldable Resins
Region Available - Global Yes
Resin Identification TPC-ET
ISO 1043
RoHS Compliance Contact Manufacturer