Material Notes:
Delrin® SC652 is a medium viscosity acetal homopolymer, with an advanced system of lubricants. It is developed for parts requiring low wear, low friction and low squeak noise for the healthcare industry.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa

@Temperature 23.0 °C
9430 psi

@Temperature 73.4 °F
ISO 527
Elongation at Yield 11 %

@Temperature 23.0 °C
11 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 3.00 GPa

@Temperature 23.0 °C
435 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Additive Lubricant
Appearance Natural Color
Features Creep Resistance, Good
Friction, Low
Homopolymer
Lubricated
Viscosity, Medium
Wear Resistance, Good
Forms Pellets
Generic Acetal (POM) Homopolymer
Material Status Current
Part Marking Code >POM-S<
ISO 11469
Processing Method Injection Molding
Product Category Healthcare Resins
Low Wear and Friction Resins
Unreinforced Resins
Region Available - Global Yes
Resin Identification POM-S
ISO 1043
RoHS Compliance Contact Manufacturer
Uses Conveyors
Gears
Medical Applications
Parts, Engineering