Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
X-ray Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400XRD NC010 is a filled medium viscosity acetal copolymer for injection molding. It is detected in x-ray detectors. It has been developed for consideraInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
Viscosity 98000 cP

@Shear Rate 5000 1/s,
Temperature 220 °C
98000 cP

@Shear Rate 5000 1/s,
Temperature 428 °F
ISO 11403-1 -2
108000 cP

@Shear Rate 5000 1/s,
Temperature 205 °C
108000 cP

@Shear Rate 5000 1/s,
Temperature 401 °F
ISO 11403-1 -2
120000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
120000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
ISO 11403-1 -2
372000 cP

@Shear Rate 500 1/s,
Temperature 220 °C
372000 cP

@Shear Rate 500 1/s,
Temperature 428 °F
ISO 11403-1 -2
455000 cP

@Shear Rate 500 1/s,
Temperature 205 °C
455000 cP

@Shear Rate 500 1/s,
Temperature 401 °F
ISO 11403-1 -2
554000 cP

@Shear Rate 500 1/s,
Temperature 190 °C
554000 cP

@Shear Rate 500 1/s,
Temperature 374 °F
ISO 11403-1 -2
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ISO 527-1/-2
Elongation at Break 24 %
24 %
Nominal; ISO 527-1/-2
Elongation at Yield 8.0 %
8.0 %
ISO 527-1/-2
Tensile Modulus 3.20 GPa
464 ksi
ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Melting Point 168 °C
334 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >POM-XD<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM-XD
ISO 1043