Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® 500CL BK601 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 500CL BK601 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant designed for low wear and friction against metals.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 67.0 MPa
9720 psi
ISO 527-1/-2
Elongation at Break 18 %
18 %
Nominal; ISO 527-1/-2
Elongation at Yield 13 %
13 %
ISO 527-1/-2
Tensile Modulus 3.20 GPa
464 ksi
ISO 527-1/-2
Flexural Modulus 2.90 GPa
421 ksi
ISO 178
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179/1eA
0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Part Marking Code >POM<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM
ISO 1043
UL recognition UL