Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® SK601 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® SK601 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 BK851 is a 10% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 4.50 GPa
653 ksi
ISO 527-1/-2
Flexural Strength 140 MPa
20300 psi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179/1eU
3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 20 %
20 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Comparative Tracking Index 250 V
250 V
IEC 60112
Descriptive Properties Value Comments
Emission of organic compounds 72 µgC/g
VDA 277
Part Marking Code >PBT-GF10<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PBT-GF10