Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® PC164 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® PC164 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for the Healthcare Industry Crastin PC164 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection molding. It has been developed for consideration into appInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
ISO 527-1/-2
Elongation at Break 30 %
30 %
Nominal; ISO 527-1/-2
Elongation at Yield 6.0 %
6.0 %
ISO 527-1/-2
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-1/-2
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >PBT<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PBT