Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® LW9320LM BK591 PBT+SAN  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® LW9320LM BK591 PBT+SAN  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has excellent surface aspect dimensional stability and loInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527-1/-2
Elongation at Break 2.3 %
2.3 %
ISO 527-1/-2
Tensile Modulus 7.30 GPa
1060 ksi
ISO 527-1/-2
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Part Marking Code >PBT+SAN-GF20<
ISO 11469
Processing Injection Moulding
Regional Availability North America
South and Central America
Resin Identification PBT+SAN-GF20