Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Crastin® LW9030 BK851 PBT+ASA  (Unverified Data**)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + ASA Blend, Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Crastin® LW9030 BK851 PBT+ASA  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 BK851 is a 30% glass fiber reinforced black polybutylene terephthalate blend for injection molding. It has improved surface aesthetics excellent dimenInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
ISO 527-1/-2
Tensile Modulus 9.20 GPa
1330 ksi
ISO 527-1/-2
Flexural Strength 180 MPa
26100 psi
ISO 178
Flexural Modulus 8.50 GPa
1230 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
ISO 180/1A
7.00 kJ/m²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180/1U
50.0 kJ/m²

@Temperature -30.0 °C
23.8 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
4.50 J/cm²

@Temperature -30.0 °C
21.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179/1eA
0.700 J/cm²

@Temperature -30.0 °C
3.33 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 170 °C
338 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 20 %
20 %
ISO 4589-1/-2
Descriptive Properties Value Comments
Part Marking Code >PBT+ASA-GF30<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PBT+ASA-GF30
UL recognition UL