Material Notes:
Nucrel® Nucrel® AE is a terpolymer of ethylene, methacrylic acid, and acrylate, available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins. It can be used as a blend of approximately 20 to 40% Nucrel® AE with 80 to 60% LDPE for enhancement of foil adhesion properties. The level of adhesion improvement depends on processing conditions.Characteristics:Improved foil adhesion when processed under the correct conditionsIncreased peak hot tack strength. Applications:Foil-containing pouches and sachets for packaging non-aggressive food and miscellaneous non-food products Snack structures Other foil, metallized film, or paper coatings as a heat seal or tie layer Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 80.0 °C
176 °F
Freezing Point, DSC; ASTM D3418
105 °C
221 °F
DSC; ASTM D3418
Vicat Softening Point 79.0 °C
174 °F
ASTM D1525