DuPont Keldax® 6705B Filled Thermoplastic Ethylene Polymer

Category Polymer , Thermoplastic
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Keldax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Keldax® 6705B Filled Thermoplastic Ethylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A filled thermoplastic ethylene polymer that provides acoustical sound barrier performance in automotive, construction, and industrial applications.Processing Method: ExtrusionSheetAvailability: North AmericaInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792 - ISO 1183
Melt Index of Compound 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ASTM D2240 - ISO 868
Tensile Strength at Break 1.03 MPa
150 psi
ASTM D638 - ISO 527-2
Elongation at Break 350 %
350 %
ASTM D638 - ISO 527-2