Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Fusabond® N493 Polymer Modifier

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer DuPont
Trade Name Fusabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Fusabond® N493 Polymer Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Fusabond® N493 is an anhydride modified ethylene copolymer. DuPont™ Fusabond® N493 can only be used in the following applications: all polyamide blends and blends for golf balls and blends for "compatibilizing flame retardant fillers for in non-halogen flame retardant polyolefin-based wire and cable compounds" Used in wire and cable applications as a polymer modifier
Physical Properties Metric English Comments
Density 0.870 g/cc
0.0314 lb/in³
ASTM D792, ISO 1183
Melt Flow 1.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 28.0 °C
82.4 °F
Freezing Point; ASTM D3418
50.0 °C
122 °F
ASTM D3418, ISO 3146
Processing Properties Metric English Comments
Processing Temperature <= 290 °C
<= 554 °F
Users viewing this material also viewed the following: