DuPont™ Fusabond® E265 Polymer Modifier

Category Polymer , Thermoplastic , Adhesives, Sealants, and Coatings
Manufacturer DuPont
Trade Name Fusabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Fusabond® E265 Polymer Modifier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Fusabond® E265 is an anhydride modified high density polyethylene. Used as a polymer modifier
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792, ISO 1183
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 111 °C
232 °F
Freezing Point; ASTM D3418
131 °C
268 °F
ASTM D3418, ISO 3146
Processing Properties Metric English Comments
Processing Temperature <= 290 °C
<= 554 °F