DuPont Elvax® 3165LG Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvax® 3165LG Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Elvax® 3165XZ is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applications: This resin is designed to provide a low temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blown film equipment over a wide range of film thickness and blow-up ratios. It can also be coextruded with a variety of other polymers. This resin is typically used as low temperature seal layer in coextruded films.Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792, ISO 1183
Vinyl Acetate Content 18 %
18 %
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 68.0 °C
154 °F
Freezing Point; ASTM D3417
89.0 °C
192 °F
ASTM D3417
Vicat Softening Point 69.0 °C
156 °F
ASTM D1525, ISO 306