Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Elvaloy® 4924 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvaloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvaloy® 4924 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792 - ISO 1183
Melt Flow 7.0 - 23 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 - 23 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.90 MPa
1581 psi
ASTM D638 - ISO 527-2
Elongation at Break 736 %
736 %
ASTM D638 - ISO 527-2
Thermal Properties Metric English Comments
Melting Point 70.0 °C
158 °F
ASTM D3418 - ISO 3146
Glass Transition Temp, Tg -36.0 °C
-32.8 °F
ASTM D3418
Users viewing this material also viewed the following: