DuPont™ Clysar® RS900 Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyolefin , Polyolefin, Film Grade , Polyolefin, Film Grade (Polyolefin)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Clysar® RS900 Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by DuPont Packaging Polymers.A strong, clear, permeable antifog shrink film engineered for food packaging. It forms tight, leak-resistant heat seals. Printable grades (RST900) offer good ink adhesion without the use of primers. Designed for appealing presentation of food products in refrigerated retail displays. Typical products include fresh trayed meat case items like poultry, meats, fish, and sausage, as well as fruit and produce.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.360 cc-mm/m²-24hr-atm
0.914 cc-mil/100 in²-24hr-atm
ASTM 1249
Water Vapor Transmission 24.0 g/m²/day
1.55 g/100 in²/day
ASTM 1249
Oxygen Transmission 212 cc-mm/m²-24hr-atm
538 cc-mil/100 in²-24hr-atm
or 14100 cc/m²-24hr-atm for the film. ASTM D3985
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 150 %
150 %
Average; ASTM D882
Modulus of Elasticity 0.190 GPa
27.6 ksi
(stiffness), ASTM D882
Coefficient of Friction, Dynamic 0.30
0.30
ASTM D1894
Seal Strength 2300 g/25 mm
2300 g/in
F-88-68(73)
Film Tensile Strength at Break, MD 76.0 MPa
11000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 4.0 %
4.0 %
Gloss 120 %
120 %