Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Biomax® 800C Hydro/Biodegradable Polyester  (discontinued **)

Category Polymer , Film , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Biomax® 800C Hydro/Biodegradable Polyester  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fully degradable polymer based on PET polyester technology. It is suited for single-use products such as films for food packaging, paper coating, injection molding uses, and thermoforming. Products made from Biomax® offer significant environmental benefits such as: hydro/biodegradable, no adverse environmental effects during or after degradation, and compatibility with all municipal solid waste disposal methods (landfill, incineration, composting, recycling).Information provided by DuPont Polyester Resins & Intermediates.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 40 - 50 %
40 - 50 %
Orientation not specified
Secant Modulus 0.0620 - 2.10 GPa
8.99 - 305 ksi
for film
Film Tensile Strength at Break, MD 13.8 - 48.3 MPa
2000 - 7010 psi
Orientation not specified
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F