Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials including APET, PETG, PP, PS, HIPS, and PVC. Appeel® 1184 is a modified ethylene acrylate polymer available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene resins. Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Viscosity 1.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
1.00e+6 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Seal Strength 1500 g/25 mm
1500 g/in
PP, bar temp 150-175°C
4000 g/25 mm
4000 g/in
HDPE, bar temp 150-175°C
Thermal Properties Metric English Comments
Melting Point 65.0 °C
149 °F
Freezing Point via DSC/ASTM D3418
85.0 °C
185 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 53.0 °C
127 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 275 °C
527 °F
Typical extrusion metering zone. May be extruded up to 300°C.
Nozzle Temperature 275 °C
527 °F
Die
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved