Dow VORANOL™ CP 3131 Polyol

Category Polymer , Thermoset
Manufacturer Dow Chemical
Trade Name VORANOL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow VORANOL™ CP 3131 Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VORANOL™ CP 3131 polyol is a low to medium reactivity polyether triol, especially designed for the production of hot molded polyurethane flexible foams.Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
pH 7.5 - 9.5
7.5 - 9.5
(1 Water / 10 Methanol); DOWM 101495-TE94A
Viscosity Measure 250 cSt

@Temperature 37.8 °C
250 cSt

@Temperature 100 °F
ASTM D445-94
470 - 515 cSt

@Temperature 25.0 °C
470 - 515 cSt

@Temperature 77.0 °F
ASTM D445-94
1470 cSt

@Temperature 10.0 °C
1470 cSt

@Temperature 50.0 °F
ASTM D445-94
Maximum Moisture Content 0.060
0.060
wt% water; ASTM E203-96
ASTM Color <= 30
<= 30
APHA; ASTM D4890-93
Thermal Properties Metric English Comments
Flash Point 236 °C
457 °F
DIN 51758
Chemical Properties Metric English Comments
Total Acid Number <= 0.050
<= 0.050
[mg KOH/g]; DOWM 100387-TE95A
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 54 - 58
ASTM D4274-94d