Dow Tyrin® CM674 Elastomer Formulation

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Dow Chemical
Trade Name Tyrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Tyrin® CM674 Elastomer Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationTyrin® CPE Elastomer
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Volatiles <= 0.20 %
<= 0.20 %
100783-LE90A
Viscosity 1.25 cP

@Shear Rate 144 1/s,
Temperature 190 °C
1.25 cP

@Shear Rate 144 1/s,
Temperature 374 °F
Melt Viscosity; CPE D-3A
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.3 MPa
1490 psi
DOWM 100789-LE90A
Elongation at Break 800 %
800 %
DOWM 100789-LE90A
100% Modulus 0.00340 GPa
0.493 ksi
DOWM 100789-LE90A
Thermal Properties Metric English Comments
Heat of Fusion 33.47 J/g
14.40 BTU/lb
DOWM 100789-LE90A
Descriptive Properties Value Comments
Chlorine Content 25 wt%
CPE D-6a