Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow SE PB-5800 Low-cis polybutadiene rubber (lithium-catalyzed) for plastics modification.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SE PB-5800 is a low-cis polybutadiene synthetic rubber. It is produced by anionic solution polymerization which affords polymers with very controlled micro- and macrostructure. SE PB-5800 is translucent to white in appearance and contains a non-staining stabilizer which complies with compositional requirements of the food packaging regulations of European countries and the USA. SE PB-5800 is used to manufacture toughened polystyrene or ABS, supporting grafting processes with its content of reactive vinyl groups. SE PB-5800 is supplied in bales weighing 30 kg. Bales are wrapped in 70 micron polystyrene film. Information provided by Dow
Physical Properties Metric English Comments
Viscosity Measurement 175
175
[mPa·s]; in 5% mass in styrene solution; ASTM D445
Mooney Viscosity 50

@Temperature 100 °C
50

@Temperature 212 °F
[MU]; ML 1+4; ASTM D1646
Vinyl Acetate Content 11 %
11 %
Supplier Method (FTIR)
Ash 0.050 %
0.050 %
ASTM D5667
Collected Volatile Condensable Material 0.40 %
0.40 %
ASTM D5668
ASTM Color 5.0
5.0
[APHA]; Supplier Method
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
Descriptive Properties Value Comments
Cis-1,4 Content % 37
Supplier Method (FTIR)
Wet Gel Index 1.5
Supplier Method