Dow R7021-50RNA Polypropylene Random Copolymer Resin

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded , Polypropylene, Molded
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow R7021-50RNA Polypropylene Random Copolymer Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW™ R7021-50RNA Polypropylene Resin is a random copolymer designed for thin wall injection molding applications desiring high clarity.Main CharacteristicsGood impact propertiesExcellent opticsFast cycle timesContains clarifier and antistat additivesComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Index of Compound 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus, 1% Secant 1070 MPa
155000 psi
ASTM D790A
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C
172 °F
Unannealed; ASTM D648
Optical Properties Metric English Comments
Haze 5.0 %
5.0 %
508 microns; ASTM D1003
14 %
14 %
1020 microns; ASTM D1003