Material Notes:
PRIMACOR® 3150 polymer containing 3% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion to metallic, paper and polyethylene substrates, and offers good drawdown, heat sealability and oil/grease resistance. When used unmodified for food packaging applications, this resin complies with the U.S. Food, Drug and Cosmetic Act as amended under Food Additive Regulation 21 CFR 177.1310(b). This resin will also comply with 21 CFR 175.105, 176.170(b), 176.180, and 178.1005. The regulations should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
Melt Flow 11 g/10 min

@Load 2.16 kg
11 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.3 MPa
1780 psi
Tensile Strength, Yield 8.80 MPa
1280 psi
Elongation at Break 585 %
585 %
Thermal Properties Metric English Comments
Vicat Softening Point 88.9 °C
192 °F