Dow Nordel® NDR 47085.03 EPDM Hydrocarbon Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name Nordel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Nordel® NDR 47085.03 EPDM Hydrocarbon Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NDR 47085.03 is a developmental product in granular form which contains carbon black. NDR 47085.03 is a high molecular weight semicrystalline EPDM grade. It offers fast cure rates and high states of cure with standard sulfur cure systems. This product is suited for applications such as extruded profiles, hose and sheeting.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D297
Volatiles <= 0.40 %
<= 0.40 %
Total Volatiles; DuPont Dow EPRG-21
Mooney Viscosity 108

@Temperature 125 °C
108

@Temperature 257 °F
ML 1 + 4; ASTM D1646
Descriptive Properties Value Comments
Carbon Black Content (N650) 30 phr
DuPont Dow EPRG-2
ENB 4.5 mass%
ASTM D6047
Ethylene 69.5 mass%
ASTM D3900
Propylene 26 mass%
ASTM D3900