Material Notes:
FormulationNordel® IP 4770R
Physical Properties Metric English Comments
Density 1.064 g/cc
0.03844 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Vulcanizate, Press cured, TC95 +3min at 180°C
Tensile Strength, Ultimate 26.1 MPa
3790 psi
Vulcanizate, Press cured, TC95 +3min at 180°C
Elongation at Break 266 %
266 %
Vulcanizate, Press cured, TC95 +3min at 180°C
100% Modulus 0.00560 GPa
0.812 ksi
Vulcanizate, Press cured, TC95 +3min at 180°C
200% Modulus 0.0170 GPa
2.47 ksi
Vulcanizate, Press cured, TC95 +3min at 180°C
Tear Strength 30.6 kN/m
175 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 180°C
Compression Set 61 %

@Temperature 125 °C
61 %

@Temperature 257 °F
Pellets cured MDR t'95 + 15 min, 70 hr; Method B
Thermal Properties Metric English Comments
Brittleness Temperature -28.0 °C
-18.4 °F
Temperature Retraction, TR-10