Dow Latex XZ 92240.03 Experimental Latex

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Dow Chemical
Trade Name Latex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Latex XZ 92240.03 Experimental Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: XZ 92240.03 Experimental latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as a precoat /adhesive latex for secondary backing of tufted carpet where a medium handle is required.Applications: Precoating and Secondary backingInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 50 - 51 %
50 - 51 %
Particle Mesh Size 100 Mesh
100 Mesh
<0.1 g/l residues
325 Mesh
325 Mesh
<0.2 g/l residues
pH 7.2 - 7.6
7.2 - 7.6
Brookfield Viscosity 50 - 350 cP
50 - 350 cP
#2 @ 50 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 2.00 °C
35.6 °F
Descriptive Properties Value Comments
Minimum film formation temperature <0°C
Styrene content in polymer 0.58