Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow LDPE 510I Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 510I Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW LDPE 510I resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate flexibility, for caps/closures, etc. It has good processability over a wide range of molding conditions. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. The regulation should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
Viscosity 76000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
76000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
176000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
176000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
305000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
305000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 2.0 g/10 min

@Load 2.16 kg
2.0 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.1 MPa
1900 psi
Tensile Strength, Yield 10.7 MPa
1550 psi
Elongation at Break 480 %
480 %
Modulus of Elasticity 0.193 GPa
28.0 ksi
Molded Sample 2% Secant Modulus
Izod Impact, Notched (ISO) 69.4 kJ/m²

@Temperature -50.0 °C
33.0 ft-lb/in²

@Temperature -58.0 °F
Tensile Impact Strength 315 kJ/m²
150 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
Users viewing this material also viewed the following: