Dow INTEGRAL™ 925 High Heat Multilayer Adhesive Film

Category Polymer , Film , Thermoset
Manufacturer Dow Chemical
Trade Name INTEGRAL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INTEGRAL™ 925 High Heat Multilayer Adhesive Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INTEGRAL 925 High Heat Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, fiberglass, non-wovens, and rigid urethanes.Information provided by Dow
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 450 %
450 %
ASTM D882
Film Elongation at Break, TD 500 %
500 %
ASTM D882
Secant Modulus, MD 0.207 GPa
30.0 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.207 GPa
30.0 ksi
2% Secant; ASTM D882
Elmendorf Tear Strength, MD 5.91 g/micron
150 g/mil
ASTM D882
Elmendorf Tear Strength, TD 17.7 g/micron
450 g/mil
ASTM D882
Film Tensile Strength at Break, MD 35.9 MPa
5200 psi
ASTM D882
Film Tensile Strength at Break, TD 26.9 MPa
3900 psi
ASTM D882