Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow INSPIRE™ DT701-14 TPO  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INSPIRE™ DT701-14 TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Flow, High Impact TPOInformation provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 14 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 0.895 GPa
130 ksi
ASTM D790A
Izod Impact, Notched NB
NB
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
Unannealed; ASTM D648