Dow INSPIRE™ D500.00 Developmental Performance Polymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Dow Chemical
Trade Name INSPIRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INSPIRE™ D500.00 Developmental Performance Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
D 500.00 Developmental Performance Polymer is a performance plastic designed for cut sheet thermoforming. The propylene-based polymer offers improved formability in large part thermoforming applications. It has melt strength specifically suited to the thermoforming process, improved sheet sag / drape performance, low temperature toughness, high chemical resistance, better regrind capability without significant loss of properties.Information provided by Dow
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Melt Flow 0.45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D882
Flexural Modulus 2.00 GPa
290 ksi
Tangent; ASTM D790A
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D256
1.07 J/cm

@Temperature -18.0 °C
2.00 ft-lb/in

@Temperature -0.400 °F
ASTM D256
Falling Dart Impact 21.0 J
15.5 ft-lb
@ 23°C, 3.4 m/s; ASTM D3763
31.0 J
22.9 ft-lb
@ -18°C, 3.4 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
22.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.3 °C
137 °F
Unannealed; ASTM D648