Material Notes:
INSPIRE 404 Performance Polymer is a propylene-based resin intended for use in thermoforming applications where exceptional stiffness, clarity and heat resistance is desired. The high stiffness of the resin may allow for the potential to down gauge and reduce part weight. The product is well suited for thin wall containers, serviceware and closure applications such as clear drink cups, deli containers, take-out containers, bowls and clear lids. It contains a nucleating agent, it is an excellent balance of stiffness and clarity, it has superior heat resistance over conventional polypropylene, and it complies with U.S. FDA 21 CFR 177.1520(c)3.2a (with Restrictions)Information provided by Dow
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.1 MPa
6100 psi
ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
1% Secant; ASTM D790B
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
264 °F
unannealed; ASTM D648
Optical Properties Metric English Comments
Haze 16 %

@Thickness 1.00 mm
16 %

@Thickness 0.0394 in
ASTM D1003