Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow INSPIRE™ 117.00 Performance Polymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Dow Chemical
Trade Name INSPIRE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INSPIRE™ 117.00 Performance Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
117.00 Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistance, and clarity are required. It has outstanding heat resistance, excellent balance of high stiffness and toughness, and good contact clarity and gloss, low taste & odor transfer. It contains a nucleating agent and it Complies with U.S. FDA 21 CFR 177.1520.Information provided by Dow
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.8 MPa
4900 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
1% Secant; ASTM D790A
Izod Impact, Notched 5.61 J/cm
10.5 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
240 °F
unannealed; ASTM D648