Material Notes:
DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent processability over a wide range of molding conditions. Typical applications are thin wall containers, overcaps, and general purpose applications. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
Viscosity 48000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
48000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
73000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
73000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
105000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
105000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 30 g/10 min

@Load 2.16 kg
30 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.0 MPa
1600 psi
Tensile Strength, Yield 22.1 MPa
3210 psi
Elongation at Break 400 %
400 %
Modulus of Elasticity 0.759 GPa
110 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 1.21 GPa
175 ksi
Izod Impact Resistance 3.20 J/cm²
15.2 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
Users viewing this material also viewed the following: