Material Notes:
DOWLEX® 3010 Polyethylene resin is a polyethylene polymer designed to offer high performance properties such as excellent environmental stress crack resistance, tear strength, abrasion resistance, and strong heat seals in thin extrusion coatings. It has good processability over a wide range of molding conditions. This material complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 for food contact applications and with regulation 177.1390 c (1) (I) (a) for high temperature laminates. The regulations should be consulted for complete details.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
Melt Flow 5.5 g/10 min

@Load 2.16 kg
5.5 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 7.5.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 14.5 MPa
2100 psi
Tensile Strength, Yield 12.4 MPa
1800 psi
Elongation at Break 720 %
720 %