Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow DOWLEX™ 2071 Linear Low Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Dow Chemical
Trade Name DOWLEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow DOWLEX™ 2071 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks and trash bags. It contains high level of slip additive and medium level of antiblock additive. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.1 (a) for food packaging applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 38 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
Thickness 38.0 microns
1.50 mil
Melt Flow 0.85 g/10 min

@Load 2.16 kg
0.85 g/10 min

@Load 4.76 lb
Melt flow ratio I10/I2 is 8.5.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 13.0 MPa
1890 psi
Film Tensile Strength at Yield, TD 15.0 MPa
2180 psi
Coefficient of Friction 0.20
0.20
Elmendorf Tear Strength MD 350 g
350 g
Elmendorf Tear Strength TD 940 g
940 g
Elmendorf Tear Strength, MD 9.20 g/micron
234 g/mil
Elmendorf Tear Strength, TD 24.7 g/micron
627 g/mil
Dart Drop 5.90 g/micron
150 g/mil
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
Film Tensile Strength at Break, TD 31.0 MPa
4500 psi
Thermal Properties Metric English Comments
Vicat Softening Point 112 °C
234 °F
Optical Properties Metric English Comments
Haze 10 %
10 %
Gloss 28 %
28 %
45°
Processing Properties Metric English Comments
Processing Temperature 226 °C
439 °F
Film extrusion temperature