Dow Corning Z-6697 SILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6697 SILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tetraethoxysilane (TEOS, Si(OC2H5)4) - diluent for zinc-rich primers, additive for other coupling agents.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc

@Temperature 25.0 °C
0.930 g/cc

@Temperature 77.0 °F
Volatile Organic Compounds (VOC) Content 751 g/l
751 g/l
Molecular Weight 208 g/mol
208 g/mol
Thermal Properties Metric English Comments
Flash Point >= 45.0 °C
>= 113 °F
closed cup
Component Elements Properties Metric English Comments
SiO2 28.7 %
28.7 %
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Active Content (%) 99
Appearance clear liquid